Related Experiment Video
Updated: Jun 13, 2025

A Uniaxial Compression Experiment with CO2-Bearing Coal Using a Visualized and Constant-Volume Gas-Solid Coupling Test System
Published on: June 12, 2019
Surface damage reduction effect of ultra-high working face in Shangwan coal mine
L I U Xinjie1, Yang Yingming2, Zhao Yongqiang2
1State Key Laboratory of Water Resource Protection and Utilization in Coal Mining, National Institute of Clean-and -Low-Carbon Energy, Beijing, 102209, People's Republic of China. liuxinjie@pku.edu.cn.
Abstract:
Green mining is the basic background of high-quality mining, and source reduction is the most important part, among which the optimization of working face height and length is the most active. How to control the working face parameters, reasonably evaluate the surface subsidence characteristics of the super-long working face, and identify the limit working face length and the surface discontinuous deformation threshold is particularly important. In order to solve the problem of irreversible damage to the surface caused by the mining process of the working face, this paper discusses the whole process of surface movement in the 8.8 m super-large mining height working face of Shangwan Coal Mine through field investigation, the maximum subsidence is 6.20 m, with a subsidence coefficient of 0.72. Combined with the inflection point trajectory, advancing degree and subsidence coefficient, the 0.9 coefficient of the working face subsidence basin boundary and the loss reduction strategy far from the limit working face threshold are proposed. The results show that the subsidence basin of 12,401 working face accounts for 34%, the continuous deformation area of surface accounts for 64%, and the influence area of discontinuous deformation area is within 10 times of mining height. With the help of borehole detection verification, the caving zone height within the coal seam overburden to be between 33.2 and 33.25 m and the fracture zone height between 118.08 and 132.83 m. Therefore, the caving ratio is about 3.8, and the fracture ratio is about 13-15, which provides a strong basis for the optimization design of working face and the timing of surface ecological management.
Related Concept Videos
Quarrying of Stone
One common method involves using a diamond belt saw to cut large blocks from the quarry face. These blocks can be about 50 feet long and 12 feet high. After the initial vertical cut, drilling is performed at the base of the...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Wood Surfacing
The equipment used in the surfacing process is a plane equipped with rotating blades. This tool efficiently smoothens the wood surface and can...