Abstract:
The synthesis of a vanadium dioxide (VO2) film using atomic layer deposition (ALD) with vanadium tetrachloride (VCl4) as a precursor for the realization of programmable memory devices is reported. X-ray diffraction analysis revealed the epitaxial growth of VO2 on c-Al2O3. The phase transition was monitored using resistivity measurements across varying temperatures, demonstrating a decrease of >4 orders of magnitude at the transition temperature, thereby confirming the high quality of the material. From this material, memristive devices are fabricated as resistive random-access memory (RRAM). On the basis of spiking voltage inputs, these RRAM exhibited cycle stability over 512 cycles and state retention stability for >450 s, showing <2% drift. With respect to synaptic-like applications, the RRAM devices were piloted through step patterns to enable multilevel memory states. These ALD-grown VO2-based devices demonstrate potential for use as synaptic connections with multiweight synapses, advancing scalability in neuromorphic applications.
More Related Videos
09:49In Situ Transmission Electron Microscopy with Biasing and Fabrication of Asymmetric Crossbars Based on Mixed-Phased a-VOx
Published on: May 13, 2020
10:40A Fabrication and Measurement Method for a Flexible Ferroelectric Element Based on Van Der Waals Heteroepitaxy
Published on: April 8, 2018