Strength degradation characteristics and damage constitutive model of sandstone under freeze-thaw cycles

Zhongwen Wang1,2, Meilu Yu3,4, Lei Wang1

  • 1State Key Laboratory of Mining Response and Disaster Prevention and Control in Deep Coal Mines, Anhui University of Science and Technology, Huainan, 232001, Anhui, China.

Scientific Reports
|September 30, 2024
PubMed

Related Concept Videos

Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
93
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
98
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
75
Stress-Strain Diagram - Brittle Materials01:24

Stress-Strain Diagram - Brittle Materials

Brittle materials, including glass, cast iron, and stone, exhibit unique characteristics. They fracture without considerable change in their elongation rate, indicating that their breaking and ultimate strength are equivalent. Such materials also show lower strain levels at the point of rupture. The failure in brittle materials predominantly results from normal stresses, as evidenced by the rupture created along a surface perpendicular to the applied load. These materials do not display...
2.2K
Brick Durability, Strength, and Appearance01:15

Brick Durability, Strength, and Appearance

Brick durability, strength, and appearance are crucial factors in construction, influencing the choice of bricks for specific applications. The process of freeze-thaw, for instance, significantly affects brick durability. This phenomenon occurs when water absorbed by a brick expands as it freezes, potentially causing damage when it melts and refreezes. Bricks are graded for durability: SW-grade bricks are the most durable, offering high strength and low water absorption, followed by MW-grade...
164
Fatigue Strength of Concrete01:22

Fatigue Strength of Concrete

Fatigue, in the context of materials science and engineering, refers to the weakening or failure of a material caused by repeatedly applied loads, even if these loads are below the strength limit of the material. Fatigue strength in concrete is a critical property that influences its durability and longevity. Concrete can fail in two ways due to fatigue. Static fatigue or creep rupture occurs under a constant load or one that increases slowly. The other failure mode is due to cyclical or...
171