Related Experiment Video
Updated: Jun 11, 2025

Preparation of Biopolymer Aerogels Using Green Solvents
Published on: July 4, 2016
From Cellulose Solutions to Aerogels and Xerogels: Controlling Properties for Drug Delivery
Loris Gelas1, Tatiana Budtova1
1Mines Paris, PSL University, Center for Materials Forming (CEMEF), UMR CNRS 7635, CS 10207, 06904 Sophia Antipolis, France.
None:
A cheap and easy-to-recycle solvent, namely, aqueous NaOH with no additives, was used to dissolve cellulose and make cross-linker-free materials with varying porosity, testing them as drug delivery devices. Cellulose solutions were gelled, coagulated in a nonsolvent (water, ethanol), and dried either using supercritical CO2 (aerogels) or low-vacuum evaporation (named "xerogels"). Aerogels had densities of around 0.1 g/cm3 and specific surface areas (SSAs) of 200-400 m2/g. A significant influence of the first nonsolvent and drying mode on material properties was recorded: when the first nonsolvent was ethanol and low-vacuum drying was performed from ethanol, aerogel-like xerogels were obtained with densities of around 0.2 g/cm3 and SSAs of 200-260 m2/g. Other conditions (under evaporative drying) resulted in cellulose with much lower porosity and SSA. All materials were evaluated as drug delivery devices in simulated gastrointestinal fluids; theophylline was used as a model drug. Materials of high porosity exhibited shrinking and rapid drug release, whereas denser materials swelled and showed slower release. Two release mechanisms were suggested: diffusion through aqueous media in pores and diffusion through swollen pore walls. The results demonstrate a large spectrum of options for tuning the properties of porous cellulose materials for drug release applications.