New Methodology for Evaluating Strength Degradation from Temperature Increase in Concrete Hydration under Adiabatic

Adelino V Lopes1, Sergio M R Lopes2

  • 1INESC, Department of Civil Engineering, University of Coimbra, 3030-788 Coimbra, Portugal.

PubMed

Related Concept Videos

Hot Weather Concreting01:20

Hot Weather Concreting

Concreting at elevated temperatures accelerates the hydration process, leading to quicker setting but potentially reducing the long-term strength of the concrete structure. Additionally, low air humidity fosters rapid moisture loss from the concrete, resulting in reduced workability, pronounced plastic shrinkage, and a higher likelihood of crazing.
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
58
Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
74
Cold Weather Concreting01:27

Cold Weather Concreting

When freshly poured concrete is exposed to freezing temperatures before it has set, the water within the concrete can freeze. This expansion disrupts the setting process, delays chemical reactions necessary for hardening, and increases the volume of pores within the hardened concrete, which weakens its overall structure. If the concrete manages to reach an appreciable strength before it freezes, the damage can be somewhat mitigated.
To counteract the negative impacts of cold weather, ensuring...
59
Mass Concreting01:22

Mass Concreting

Mass concreting refers to the process of placing large volumes of concrete, such as in gravity dams. The heat generated during the cement hydration process and differential cooling rates within the concrete mass can lead to a temperature gradient, which can result in thermal cracks in the concrete mass.
To reduce the risk of such cracking, the concrete mix may incorporate low-heat cement and pozzolans to reduce the temperature rise. Pre-cooled angular aggregates and water-reducing admixtures...
59
Fatigue Strength of Concrete01:22

Fatigue Strength of Concrete

Fatigue, in the context of materials science and engineering, refers to the weakening or failure of a material caused by repeatedly applied loads, even if these loads are below the strength limit of the material. Fatigue strength in concrete is a critical property that influences its durability and longevity. Concrete can fail in two ways due to fatigue. Static fatigue or creep rupture occurs under a constant load or one that increases slowly. The other failure mode is due to cyclical or...
171
Strength and Heat of Hydration01:29

Strength and Heat of Hydration

The hydration of cement is an exothermic reaction in which heat is generated as cement hydrates. This heat of hydration is critical to cement's strength development. The rate at which this heat is generated affects the temperature rise, with a majority of the heat being released early in the hydration process, half within the first three days, and about 75% within the first week.
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
215