Boosting Thermogalvanic Cell Performance through Synergistic Redox and Thermogalvanic Corrosion

Wei Fang1, Haoran Luo1, Ibrahim Mwamburi Mwakitawa1

  • 1MOE Key Laboratory of Low-grade Energy Utilization Technologies and Systems, School of Energy & Power Engineering, Chongqing University, Chongqing, 400044, China.

Chemsuschem
|October 18, 2024
PubMed

Related Concept Videos

Voltaic/Galvanic Cells02:47

Voltaic/Galvanic Cells

Spontaneous Chemical Reactions
Spontaneous redox reactions occur abundantly in nature. The chemical reaction occurring in a disposable AA battery powering our remote controls is one such example of a spontaneous redox reaction. Another example is the immersion of coiled copper wire into an aqueous silver nitrate solution. The reaction shows a gradual, visually impressive color change from colorless to bright blue and the formation of a grey precipitate on the copper wire. In this experiment,...
56.8K
Electrolysis03:00

Electrolysis

In a galvanic cell, the electrical work is done by a redox system on its surroundings as electrons produced by the spontaneous redox reactions are transferred through an external circuit. Alternatively, an external circuit does work on a redox system by imposing a voltage sufficient to drive an otherwise nonspontaneous reaction in a process known as electrolysis. For instance, recharging a battery involves the use of an external power source to drive the spontaneous (discharge) cell reaction in...
26.1K
Standard Electrode Potentials03:02

Standard Electrode Potentials

On comparing the reactivity of silver and lead, it is observed that the two ionic species, Ag+ (aq) and Pb2+ (aq), show a difference in their redox reactivity towards copper: the silver ion undergoes spontaneous reduction, while the lead ion does not. This relative redox activity can be easily quantified in electrochemical cells by a property called cell potential. This property is commonly known as cell voltage in electrochemistry, and it is a measure of the energy which accompanies the charge...
43.5K
Cell Potential and Free Energy02:58

Cell Potential and Free Energy

Thermodynamics of a Redox Reaction
Thermodynamics is the branch of physics dealing with the relationship between heat and other forms of energy. In an electrochemical cell, chemical energy is converted into electrical energy.
Thus, a link can be predicted between cell potential, free energy change, and the equilibrium constant for the reaction. Cell potential can also be measured as the oxidant or the reducing strength, and similar acid-base strength measures are reflected in equilibrium...
39.7K
Redox Equilibria: Overview01:23

Redox Equilibria: Overview

A reduction-oxidation reaction is commonly called a redox reaction. In a redox reaction, electrons are transferred from one species to another rather than being shared between or among atoms. The reducing agent or reductant is the species that loses electrons and gets oxidized in the process. The species that gains electrons and gets reduced in the process is the oxidizing agent or oxidant. Redox reactions are represented as two separate equations called half-reactions, where one equation...
537
Electromotive Force02:36

Electromotive Force

Electricity is generated by either electrons or ions flowing through a solution or a conducting medium. This flow of electrons or specifically electrical charge is defined as an electric current. When electrons move through a wire, they generate an electric current. It can be recalled  that in a redox reaction, electrons are lost and gained. In the spontaneous redox reaction of zinc  with copper, when zinc is immersed in a copper ion solution, a transfer of electrons from one...
25.9K