Modelling freckles and spurious grain formation in directionally solidified superalloy castings
Haijie Zhang1, Yunxing Zhao2, Wei Xiong2
1Chair for Simulation and Modelling of Metallurgy Processes, Department of Metallurgy, University of Leoben, A-8700 Leoben, Austria.
Abstract:
Segregation channels with misoriented spurious grains, known as freckles, are an unacceptable casting defect in superalloy turbine blades. A digital-twin method to predict segregation channels was proposed in our previous studies; however, the formation of spurious grains was ignored. Here, we extend the digital twin methodology by incorporating dendrite fragmentation, which is recognized as the predominant mechanism in the formation of spurious grains. The flow-induced fragmentation process has been refined to account for the timing of dendrite pinch-off. A three-phase mixed columnar-equiaxed solidification model was used to track the motion of the crystal fragments. Directional solidification experiments for superalloy casting were conducted in an industrial-scale Bridgman furnace, and the distribution of spurious grains in the freckles was metallographically analysed. Excellent simulation-experiment-agreement was achieved. Based on this study, the formation of spurious grains within the segregation channels is mainly caused by the flow-driven fragmentation mechanism. Experimentally measured freckles can be reproduced only if the timing of the dendrite pinch-off is considered.
Related Concept Videos
Metallic Solids
All metallic solids exhibit high thermal and electrical conductivity, metallic luster, and malleability....
Imperfections in Crystal Structure: Stoichiometric Point Defects
Imperfections in Crystal Structure: Non-Stoichiometric Defects