Microstructure and Phase Equilibria in BCC-B2 Nb-Ti-Ru Refractory Superalloys

Melanie K Moczadlo1, Eric A Lass1

  • 1Department of Materials Science and Engineering, University of Tennessee Knoxville, Knoxville, TN 37996, USA.

PubMed
Summary

Refractory superalloys (RSAs) with two-phase microstructures show promise for high-temperature applications. This study investigated the Nb-Ti-Ru system, revealing key phase equilibria and elemental distributions for developing advanced RSAs.