Directing SEI formation on Si-based electrodes using atomic layer deposition

Supti Das1, Anders Brennhagen1, Carmen Cavallo1

  • 1Centre for Materials Science and Nanotechnology, Department of Chemistry, University of Oslo, PO Box 1033, Blindern, 0315, Oslo, Norway. alexey.koposov@kjemi.uio.no.