Related Experiment Video
Updated: Jun 5, 2025

Preparation of Aligned Steel Fiber Reinforced Cementitious Composite and Its Flexural Behavior
Published on: June 27, 2018
Mechanical properties of fibre-reinforced geopolymer-cemented tailings used as backfill
Xueqiang Sha1, Chao Cheng1, Guoyong Pan1
1China Construction Sixth Bureau Civil Engineering Co.Ltd., Tianjin, China.
Abstract:
Backfill materials are used in underground engineering to fill voids and buried excavated parts. In this study, solid waste was utilised as a raw material mixed with different amounts of polypropylene fibres to determine the optimal sodium hydroxide content, water-solid ratio, and fibre content. The uniaxial compressive strength (UCS) of the produced backfill materials was measured, and the interfacial structures were analysed via scanning electron microscopy. The results revealed that the mechanical properties of the backfill materials were influenced in the order sodium hydroxide doping > water-solid ratio > fibre doping. The optimal material composition corresponded to a sodium hydroxide content of 3%, water-solid ratio of 0.28, and fibre content of 5 ‰. The slag produced a C-S-H gel. Meanwhile, the fly ash and gangue contained large amounts of aluminium, which formed hydrated aluminosilicates. The addition of polypropylene fibres reduced the number of internal defects in the backfill structure and increased the UCS.
More Related Videos
Related Concept Videos
Fiber Reinforced Concrete
Additives and Fillers in Concrete
The...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Fineness of Cement
Direct...
Porosity in Cement Paste
The balance of water to cement in the mix is...
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...