Efficient Load-Bearing Capacity Assessment of a Degraded Concrete Manhole Using Sectional Homogenization
Tomasz Garbowski1, Tomasz Grzegorz Pawlak2, Anna Szymczak-Graczyk2
1Department of Biosystems Engineering, Poznan University of Life Sciences, Wojska Polskiego 50, 60-627 Poznan, Poland.
Abstract:
This study addresses a practical and efficient approach to evaluating the load-bearing capacity of severely degraded concrete manholes. Concrete deterioration, often advanced and highly irregular, can be captured accurately through surface scanning to create a detailed model of the damaged structure and also to build a simplified modeling to enable rapid engineering-level assessment, filling a critical gap in infrastructure maintenance. The repair strategy involves applying an internal polyurea layer, a variable-thickness polyurethane foam layer depending on the degree of localized degradation, and an external polyurea layer to restore the original shape of the manhole. However, these repairs do not fully restore the manhole's original load-bearing capacity. A full 3D model, encompassing millions of finite elements, would provide a detailed analysis of strength reductions but is impractical for engineering applications due to computational demands. An alternative approach utilizing sectional homogenization is proposed, where sectional properties are sequentially averaged to calculate effective parameters. This approach enables the use of only a few hundred shell elements, each representing thousands of elements from the detailed 3D model, thus providing a rapid, engineering-level assessment of load-bearing reductions in degraded manholes. The study finds that while the repair method restores up to 76% of bending stiffness in heavily corroded sections, it does not fully recover the original load-bearing capacity.
Related Concept Videos
Slump Test
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...
Segregation in Fresh Concrete
Elasticity in Concrete
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Shrinkage in Concrete
When concrete is still in its plastic state, it can undergo a decrease in volume by about 1% of its absolute volume. This decrease is known as plastic shrinkage. It arises either...
Compacting Factor test
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...