Slip-Resistant Connections with Hot-Dip Galvanized Faying Surface Under Freeze-Thaw Cycles and/or Low Temperature

Alfonso Fuente García1, Miguel Serrano López1, Carlos López-Colina Pérez1

  • 1Polytechnic School of Engineering, Campus de Viesques, University of Oviedo, 33203 Gijón, Spain.

PubMed

Related Concept Videos

Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
92
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
74
Cold Weather Concreting01:27

Cold Weather Concreting

When freshly poured concrete is exposed to freezing temperatures before it has set, the water within the concrete can freeze. This expansion disrupts the setting process, delays chemical reactions necessary for hardening, and increases the volume of pores within the hardened concrete, which weakens its overall structure. If the concrete manages to reach an appreciable strength before it freezes, the damage can be somewhat mitigated.
To counteract the negative impacts of cold weather, ensuring...
56
Steel Fastening Techniques01:17

Steel Fastening Techniques

Steel sections can be joined together through various fastening techniques including riveting, bolting, and welding, each suitable for different structural requirements and conditions.
Rivets are cylindrical steel fasteners with a specially designed head. During application, rivets are heated until white-hot and then inserted through pre-drilled holes in the steel sections. A pneumatic hammer is used to shape the exposed end into a second head, securing the sections together.
Bolting is another...
134
Masonry in Cold and Hot Weather Conditions01:21

Masonry in Cold and Hot Weather Conditions

In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units...
80
Fatigue01:21

Fatigue

Fatigue occurs when materials rupture under repeated or fluctuating loads, even at stress levels far below their static breaking strength. It typically results in brittle failure, even for ductile materials. It is a critical consideration in designing machines and structural components subjected to repetitive or varying loads. The nature of these loadings can range from fluctuating loads like unbalanced pump impellers causing vibrations to repeatedly bending a thin steel rod wire back and forth...
172