TiO2/CoO heterostructure decorated MIL-100(Fe) by atomic layer deposition for enhanced photocatalytic oxygen
Wenhui Hu1, Zhongxin Song1, Lingna Sun1
1College of Chemistry and Environmental Engineering, Shenzhen University, Shenzhen, Guangdong 518060, P. R. China. liyli@szu.edu.cn.
Abstract:
Efficient separation of photogenerated charge carriers is essential for maximizing the photocatalytic efficiency of semiconductor materials in oxygen evolution reactions (OER). This study presents a novel trimetallic photocatalyst, MIL-100(Fe)/TiO2/CoO, synthesized through a facile microwave-assisted hydrothermal method followed by atomic layer deposition (ALD). The porous MIL-100(Fe) serves as a support for the sequential deposition of TiO2 and CoO layers via ALD, which enhances electron-hole pair separation and minimizes their recombination. Characterization using transmission electron microscopy (TEM) and X-ray photoelectron spectroscopy (XPS) confirms the uniform deposition of TiO2 and CoO layers on the MIL-100(Fe) surface. The optimized photocatalyst, processed with 20 deposition cycles of Co, exhibits exceptional photocatalytic OER performance, with an oxygen evolution rate of 558.3 μmol g-1 h-1. This enhancement in activity is attributed to the synergistic interaction between the spatially separated TiO2 and CoO cocatalysts, which facilitates efficient charge transfer and increases the number of active sites. These findings highlight the potential of ALD-fabricated heterostructures in the development of advanced photocatalysts for sustainable energy production.
More Related Videos
08:14Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited Zn1-xMgxO
Published on: July 31, 2016
06:00Solvothermal Synthesis of MIL-96 and UiO-66-NH2 on Atomic Layer Deposited Metal Oxide Coatings on Fiber Mats
Published on: June 13, 2018