Coupled effects of initial water content with refrigeration temperature and freeze-thaw cycles on dewatering of

Yajun Wu1, Ruilong Li1, Xudong Zhang1

  • 1Department of Civil Engineering, School of Mechanics and Engineering Science, Shanghai University, 99 Shangda Road, Shanghai, 200444, PR China.

Environmental Research
|January 30, 2025
PubMed

Related Concept Videos

Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
89
Cold Weather Concreting01:27

Cold Weather Concreting

When freshly poured concrete is exposed to freezing temperatures before it has set, the water within the concrete can freeze. This expansion disrupts the setting process, delays chemical reactions necessary for hardening, and increases the volume of pores within the hardened concrete, which weakens its overall structure. If the concrete manages to reach an appreciable strength before it freezes, the damage can be somewhat mitigated.
To counteract the negative impacts of cold weather, ensuring...
55
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
70
Drying Shrinkage01:21

Drying Shrinkage

When hardened concrete is exposed to air with a relative humidity of less than 100 percent, it begins to lose the free water within its capillaries. As this water evaporates, the water initially adsorbed onto the calcium silicate hydrates migrates towards these now empty spaces and eventually evaporates as well. Over time, as more water leaves, the volume of the concrete decreases, a phenomenon known as drying shrinkage.
A portion of this drying shrinkage can be reversed; if the concrete is...