Abstract:
This paper presents the results of an experimental investigation on a steel-reinforced polyurethane (SRPU) composite system with a mineral interlayer, designed for the protection of existing structures. The composite SRPU was reinforced with unidirectional steel textile embedded in polyurethane matrix PS. In the study, SRPU was applied to a brick substrate via a layer of lime- or cement-based mortar of a thickness of 3 mm, 6 mm, or 10 mm. Single-lap shear tests (SLSTs) were carried out on specimens with and without a mortar interlayer. The reference specimens without a mineral interlayer carried higher loads than the specimens with an interlayer. An increase in the interlayer thickness reduced the shear bond strength. The stiffness of the bond under shear of the tested systems was unaffected by the presence of the mineral interlayer. The mechanical properties of the applied mortars influenced the observed failure modes. The tested SRPU system demonstrated notable efficiency in monotonic testing, outperforming previously reported results.
More Related Videos
11:07Preparation of Aligned Steel Fiber Reinforced Cementitious Composite and Its Flexural Behavior
Published on: June 27, 2018
10:00Experimental Protocol to Determine the Chloride Threshold Value for Corrosion in Samples Taken from Reinforced Concrete Structures
Published on: August 31, 2017
Related Concept Videos
Reinforced Brick Masonry
To fortify brick walls...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Non-destructive Tests for Concrete Strength
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Testing Water Quality
Mortar Properties