Related Experiment Video
Updated: May 22, 2025

Sandy Soil Improvement through Microbially Induced Calcite Precipitation MICP by Immersion
Published on: September 12, 2019
Improving Lime-Based Restoration Mortars: Effect of Type and Utilization Rate of Binder and Aggregate
Tuğçe İsafça-Kaya1, Yahya Kaya1, Naz Mardani2
1Department of Civil Engineering, Faculty of Engineering, Bursa Uludag University, Bursa 16059, Turkey.
Abstract:
Lime-based mortars, frequently used in historic structures, are classified as hydraulic and non-hydraulic according to how they gain strength. In the past, various methods were used to improve the strength and durability properties of lime-based hydraulic mortars such as Khorasan mortar. Today, in studies carried out to increase the strength of lime-based mortars, the effects of binders, aggregates, and additives, which are the basic components of the mortar, are examined. In this study, the mechanical properties of Khorasan mortar mixtures, which are frequently used in the restoration of historical structures, were examined under the influence of different parameters. In particular, the effects of variables such as aggregate type and ratio (river sand and crushed brick), binder type and ratio (natural hydraulic lime, metakaolin, and blast furnace slag), and water/total dry material ratio on the strength of mortars were investigated experimentally. In the experimental study, two different aggregate types (river sand and crushed brick) were used in 1/3 and 1/2 ratios, and three different binders (natural hydraulic lime, metakaolin, and blast furnace slag) were used in different ratios. The water-to-total-dry-material ratios were set at 0.2 and 0.25. Standard test samples were then created from the prepared mortar mixtures, and their flexural and compressive strengths were assessed at 28 and 56 days. A statistical analysis of the experimental data was conducted using the Taguchi method, allowing for a detailed examination of how the different parameters influenced the strength of the mortars. Through this analysis, the optimal mixture ratios that maximized mortar strength were successfully identified.
More Related Videos
05:36Production and Analysis of Sporosarcina pasteurii Biocement Bricks Using Custom 3D-Printed Molds for Unconfined Compression Tests
Published on: March 7, 2025
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Related Concept Videos
Mortar Properties
Mortar
Aggregate Cement Ratio
Bonding and Strength of Aggregate
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...