Experimental and numerical study on post-fire self-healing concrete for enhanced durability

Ajitanshu Vedrtnam1,2,3, Martin T Palou4, Hugo Varela5

  • 1Institute of Construction and Architecture, Slovak Academy of Science, Bratislava, 84503, Slovakia. ajitanshu.m@invertis.org.

Scientific Reports
|March 22, 2025
PubMed

Related Concept Videos

Abrasion Resistance of Concrete01:23

Abrasion Resistance of Concrete

Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
89
Curing of Concrete01:20

Curing of Concrete

The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
83
Fiber Reinforced Concrete01:22

Fiber Reinforced Concrete

Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
65
Fatigue Strength of Concrete01:22

Fatigue Strength of Concrete

Fatigue, in the context of materials science and engineering, refers to the weakening or failure of a material caused by repeatedly applied loads, even if these loads are below the strength limit of the material. Fatigue strength in concrete is a critical property that influences its durability and longevity. Concrete can fail in two ways due to fatigue. Static fatigue or creep rupture occurs under a constant load or one that increases slowly. The other failure mode is due to cyclical or...
155
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
67
Effects of Air-entrainment in Concrete01:28

Effects of Air-entrainment in Concrete

Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
77