Abstract:
Protective coatings are required to address interfacial incompatibility issues in composite cathodes made from Ni-rich layered oxides and lithium thiophosphate solid electrolytes (SEs), one of the most promising combinations of materials for high energy and power density solid-state battery (SSB) applications. Herein, the preparation of conformal ZrO2 nanocoatings on a LiNi0.85Co0.10Mn0.05O2 (NCM85) cathode-active material (CAM) by atomic layer deposition (ALD) is reported and the structural and chemical evolution of the modified NCM85 upon heat treatment-a post-processing step often required to boost battery performance-is investigated. The coating properties are shown to have a strong effect on the cyclability of high-loading SSB cells. After mild annealing (≈400 °C), the CAM delivers high specific capacities (≈200 mAh g-1 at C/10) and exhibits improved rate capability (≈125 mAh g-1 at 1C) and stability (≈78% capacity retention after 200 cycles at 0.5C), enabled by effective surface passivation. In contrast, annealing temperatures above 500 °C lead to the formation of an insulating interphase that negatively affects the cycling performance. The results of this study demonstrate that the preparation conditions for a given SE/CAM combination need to be tailored carefully and ALD is a powerful surface-engineering technique toward this goal.
More Related Videos
07:13High Temperature Fabrication of Nanostructured Yttria-Stabilized-Zirconia YSZ Scaffolds by In Situ Carbon Templating Xerogels
Published on: April 16, 2017
12:18Co-localizing Kelvin Probe Force Microscopy with Other Microscopies and Spectroscopies: Selected Applications in Corrosion Characterization of Alloys
Published on: June 27, 2022