Using Differential Scanning Calorimetry to Accelerate Polymerization Catalysis: A Toolkit for Miniaturized and

Thomas M McGuire1, David Ning1, Charlotte K Williams1

  • 1Department of Chemistry, University of Oxford, Oxford OX1 3TA, U.K.

ACS Catalysis
|May 8, 2025
PubMed

Related Concept Videos

Ziegler–Natta Chain-Growth Polymerization: Overview01:17

Ziegler–Natta Chain-Growth Polymerization: Overview

Ziegler–Natta polymerization is another form of addition or chain‐growth polymerization used for synthesizing linear polymers over branched polymers. The catalyst used for polymerization is the Ziegler–Natta catalyst, named after Karl Ziegler and Giulio Natta, who developed it in 1953. This catalyst is an organometallic complex of titanium tetrachloride and triethyl aluminum, with the active form of the catalyst being an alkyl titanium compound. Using the Ziegler–Natta...
3.2K
Free-Radical Chain Reaction and Polymerization of Alkenes02:35

Free-Radical Chain Reaction and Polymerization of Alkenes

The conversion of alkenes to macromolecules called polymers is a reaction of high commercial importance. The structure of the polymer is defined by a repeating unit, while the terminal groups are considered insignificant. The average degree of polymerization represents the number of repeating units in the polymer molecule and is denoted by the subscript n.
7.6K
Polymer Classification: Stereospecificity01:26

Polymer Classification: Stereospecificity

Polymerization generates chiral centers along the entire backbone of a polymer chain. Accordingly, the stereochemistry of the substituent group has a significant effect on polymer properties. Polymers formed from monosubstituted alkene monomers feature chiral carbons at every alternate position in the polymer backbone. Relative to the predominant orientation of substituents at the adjacent chiral carbons, the polymer can exist in three different configurations: isotactic, syndiotactic, and...
2.3K
Olefin Metathesis Polymerization: Acyclic Diene Metathesis (ADMET)00:53

Olefin Metathesis Polymerization: Acyclic Diene Metathesis (ADMET)

Acyclic diene metathesis polymerization or ADMET polymerization involves cross-metathesis of terminal dienes, such as 1,8-nonadiene, to give linear unsaturated polymer and ethylene. As ADMET is a reversible process, the formed ethylene gas must be removed from the reaction mixture to complete the polymerization process.
Similar to cross-metathesis, ADMET also involves the formation of metallacyclobutane intermediate by [2+2] cycloaddition of one of the double bonds of a terminal diene with...