Oxidation Resistance Enhancement of Graphene-Oxide-Semiconductor Planar-Type Electron Sources Using Al2O3 Thin

Ren Mutsukawa1,2, Yoshinori Takao3, Hiromasa Murata2

  • 1Department of Mechanical Engineering, Materials Science, and Ocean Engineering, Yokohama National University, 79-5 Tokiwadai, Hodogaya-ku, Yokohama 240-8501, Japan.