Tribological and corrosion behavior of Al2O3 interlayer reinforced friction stir welded AA6082-T6 joints
Abousoufiane Ouis1, Mohamed I A Habba2, Mohamed M Z Ahmed3
1Mechanical Engineering Department, College of Engineering at Al-Kharj, Prince Sattam Bin Abdulaziz University, Al-Kharj, 11942, Saudi Arabia.
Abstract:
Friction stir welding (FSW) of thick extruded AA6082-T6 aluminum alloy plates presents challenges in maintaining optimal mechanical and corrosion properties. This study investigated the effects of incorporating Al₂O₃ interlayer reinforcements on the microstructural, tribological, and corrosion behaviors of FSW joints. AA6082-T6 plates were friction stir welded with Al₂O₃ interlayer strips at various levels of 0, 4, 8, and 12 vol%. The resulting joints were characterized using optical microscopy, electron microscopy, X-ray diffraction, hardness testing, potentiodynamic polarization, and pin-on-disk wear tests. The Al₂O₃ reinforcement led to grain refinement, increased dislocation density, and enhanced microstrain in the weld zone. The relative density decreased with an increase in the Al₂O₃ content. The Vickers hardness improved systematically across all thicknesses of the reinforced joints, with the highest values observed in the 12 vol% Al₂O₃ specimen. The corrosion resistance of the reinforced joints improved significantly, approaching that of the base material. The wear resistance was enhanced in the reinforced joints with 8 vol% Al₂O₃ specimen consistently showing the highest enhancement ratios under various load conditions. The incorporation of Al₂O₃ interlayer reinforcements effectively mitigated the negative effects of FSW on AA6082-T6 joints, enhancing their microstructural, mechanical, tribological, and corrosion properties. Optimal performance was achieved with 8 vol% Al₂O₃ reinforcement, balancing improvements in hardness, wear resistance, and corrosion behavior.
Related Concept Videos
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Frictional Force
Corrosion of Reinforcement
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Design Example: Deciding Thickness of Lubricating Fluid in a Shaft
To calculate the required thickness of the lubricant layer, the tangential velocity at the shaft's surface must first be determined. This velocity is calculated by converting the rotational speed to angular...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Characteristics of Dry Friction
Before the wheelbarrow starts moving, the static frictional force acts tangentially to the contact surface, opposing the force that is about to induce the motion. This frictional force prevents the...