Role of Precursor Miscibility in Area-Selective Atomic Layer Deposition
Related Experiment Video
Updated: May 15, 2026

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films
Published on: December 4, 2014
Alexander Shearer1, Yukio Cho1,2, Andreas Werbrouck1
1Department of Chemical Engineering, Stanford University, Stanford, CA, 94305, USA.
Abstract:
Area-selective atomic layer deposition (AS-ALD) is of increasing importance in nanostructure fabrication, and precursor selection is critical to realizing a successful process. This work explores the role of the precursor in achieving AS-ALD of Al2O3 on a dielectric (SiO2) in the presence of a metal (Cu/CuOx). Four different precursors-dimethylaluminum isopropoxide (DMAI), trimethylaluminum (TMA), triethylaluminum (TEA), and triisobutylaluminum (TIBA)-are tested against a benzenethiol (BT) inhibitor. BT forms monolayers on Cu, whereas on CuOx it forms a thick crystalline multilayer composed of 1D-coordination polymers of Cu-thiolate (CuBT). This work observes that DMAI provides exceptional selectivity: 22 nm of Al2O3 can be deposited on patterned substrates with 99.9% selectivity, and in the case of thick CuBT can achieve excellent pattern transfer on nanoscale patterns with well-defined material interfaces. In contrast, none of the alkylaluminum precursors show significant selectivity, a result attributed to their miscibility in the CuBT multilayer leading to its degradation. This work proposes that the miscibility of the alkylaluminum precursors depends on ligand length and structure. The results show that the ligand-dependent miscibility and subsequent degradation of CuBT impact the location of Al2O3 nucleation. This study highlights new considerations for AS-ALD process design to achieve high selectivity.
Related Concept Videos
Nuclear Transmutation
Nuclear Overhauser Enhancement (NOE)
Colloidal precipitates
Atomic Absorption Spectroscopy: Interference
Spectral interference occurs when signals from other elements or molecules overlap with the analyte signal, falsely elevating or masking the analyte's absorbance. This interference can be corrected using Zeeman,...
Deleterious Substances in Aggregate
Another type of impurity is clay and fine material that...
Leveling Effect