Catalysts Design and Atomistic Reaction Modulation by Atomic Layer Deposition for Energy Conversion and Storage
Myung-Jin Jung1, Alireza Razazzadeh1, Hasmat Khan1,2
1School of Materials Science and Engineering Pusan National University Busan Republic of Korea.
Abstract:
Atomic layer deposition (ALD) technique has emerged as a fascinating tool for the design and synthesis of heterogeneous catalysts with atomic precision for energy conversion, generation, and storage applications. Here, we demonstrate the importance of the ALD for catalyst design by citing recently reported works, in particular, the emphasis has been given to the surface/interface engineering of catalysts for improving their catalytic efficiency in energy applications. To get insight into the reaction mechanism, the ALD-based routes for catalyst synthesis may revolutionize the field of sustainable energy conversion and storage. Moreover, the synthesis of supported nanoparticles with controlled shape and size has attracted great attention in catalysis owing to their unique properties. By taking advantage of the ALD, it is possible to synthesize catalysts at the atomic scale, particularly, site-selective ALD provides tremendous opportunities in catalytic efficiency and selectivity studies. Moreover, this review illustrates diverse heterogeneous catalysts with their limitations for energy-related applications and how the ALD technique can facilitate overcoming them. Finally, we deliberate the advancement in the ALD technique on heterogeneous catalyst design, and interface engineering of catalysts, and outline future perspectives of this technology in catalysis.
More Related Videos
08:40Synthesis of Metal Nanoparticles Supported on Carbon Nanotube with Doped Co and N Atoms and its Catalytic Applications in Hydrogen Production
Published on: December 6, 2021
12:12On the Preparation and Testing of Fuel Cell Catalysts Using the Thin Film Rotating Disk Electrode Method
Published on: March 16, 2018