Atomic Layer Deposition of ZrO2 Films at High Temperatures (>350 °C) Using a Modified Cyclopentadienyl Zr Precursor
Jae Chan Park1, Chang Ik Choi1, Hongseok Jang2
1Department of Materials Science and Chemical Engineering, Hanyang University, Ansan 15588, Republic of Korea.
Abstract:
With tris(dimethylamino)cyclopentadienyl metal (CpX(NMe2)3) precursors, the optimum process temperature of atomic layer deposition (ALD) is higher for HfO2 films (∼350 °C) than ZrO2 films (∼320 °C). Since simultaneous ALD of the two films is required in HfxZr1-xO2 film processes, the optimum ALD temperatures of the two films need to be adjusted equally. The cyclopentadienyl Zr precursor (MCPZr) introduced in this study exhibits better thermal stability than that of CpZr(NMe2)3. ZrO2 films were grown using CpZr(NMe2)3 and MCPZr at 350 °C, the optimum ALD temperature of the HfO2 film using CpHf(NMe2)3, and the growth behavior and physicochemical and electrical properties were compared. The physical density was higher, and the impurity concentration was lower for the film grown using MCPZr compared to the film grown using CpZr(NMe2)3. The electrical properties of dielectric constant, leakage current, and dielectric breakdown also improved due to the improved physicochemical properties.
More Related Videos
08:14Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited Zn1-xMgxO
Published on: July 31, 2016
08:18Synthesis and Characterization of High c-axis ZnO Thin Film by Plasma Enhanced Chemical Vapor Deposition System and its UV Photodetector Application
Published on: October 3, 2015