A Comparative Study of Subcutaneous Connective Tissue Reaction to A Novel Calcium Silicate Based Cement, Biodentine
Omolbanin Shahraki1, Alireza Sarhadi2, Samira Shahraki3,4
1Infectious Diseases and Tropical Medicine Research Center, Research Institute of Cellular and Molecular Sciences in Infectious Diseases, Zahedan University of Medical Sciences, Zahedan, Iran.
Abstract:
This study aimed to evaluate the biocompatibility of newly synthesised cement (Nanodentin) in comparison with Biodentine and CEM cement. The cements were implanted in rat skin and tissue reactions were assessed after 7, 30 and 60 days. H&E staining was used to measure the inflammatory response, the number of inflammatory cells and the presence of necrosis. The agar punch method was used for the antibacterial assay. The null hypothesis was that there would be no difference in terms of inflammation between Biodentine, CEM cement and Nanodentin with negative control. All cements induced a mild to moderate inflammatory reaction at day 7, which decreased over time. Nanodentin had the lowest number of inflammatory cells and necrosis among the tested materials. Nanodentin was biocompatible and well tolerated by subcutaneous tissues and had similar or better properties than the commercially available cements. It also exhibited good antibacterial activity compared to controls.
More Related Videos
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
06:23Using Baseplating and a Miniscope Preanchored with an Objective Lens for Calcium Transient Research in Mice
Published on: June 5, 2021
Related Concept Videos
Soundness of Cement
Hydration of Cement
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...