Quasi-static and dynamic nanoindentation for mechano-chemical analysis on biodegradable polymeric nanocomposites for

Antonio de Nigris1, Domenico Gentile1, Giuseppe Peter Vanoli1

  • 1Department of Medicine and Health Sciences "V. Tiberio", University of Molise, Via De Sanctis, Campobasso, 86100, Italy.