Toward durable anti/de-icing technologies: liquid-like surfaces with engineered abrasion resistance

Yifan Yan1, Fuchao Yang1,2, Daheng Wu3

  • 1Ministry of Education Key Laboratory for the Green Preparation and Application of Functional Materials, Hubei Key Laboratory of Polymer Materials and School of Materials Science & Engineering, Hubei University, Wuhan 430062, People's Republic of China. zguo@licp.cas.cn.

Materials Horizons
|September 18, 2025
PubMed
Abstract

Related Concept Videos

Abrasion Resistance of Concrete01:23

Abrasion Resistance of Concrete

Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
522
Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
400
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
377
Air-entraining Agents01:27

Air-entraining Agents

Air-entraining agents improve the durability and workability of concrete in climates with frequent freezing and thawing. These agents prevent cracks by introducing small air bubbles into the mix, creating spaces accommodating water expansion when temperatures drop. The air-entraining agents lower the surface tension of water, forming stable, small air bubbles. This method is more effective than having accidental large voids, as the intentional, smaller, and evenly distributed air voids improve...
255
Dry Friction01:30

Dry Friction

Dry friction occurs between two solid surfaces in contact as they attempt to move relative to one another. In daily life, dry friction is encountered in various forms, such as when walking on the ground, sliding an object across a table, or rubbing hands together. Despite its ubiquity, the underlying mechanisms behind dry friction are not readily visible.
To illustrate this concept, imagine a wooden crate resting on a rough, non-uniform horizontal surface. When an external force is applied to...
931
Characteristics of Dry Friction01:21

Characteristics of Dry Friction

Dry friction occurs when two solid surfaces slide against each other without any lubrication or fluid present. It causes resistance when pushing objects along a surface, like a gardener pushing a wheelbarrow. The force applied to move the cart causes dry friction between the wheel and the ground.
Before the wheelbarrow starts moving, the static frictional force acts tangentially to the contact surface, opposing the force that is about to induce the motion. This frictional force prevents the...
963