Related Experiment Video
Updated: Jan 16, 2026

Immobilization of Multi-biocatalysts in Alginate Beads for Cofactor Regeneration and Improved Reusability
Published on: April 22, 2016
Catalyst in-situ regeneration for polychlorinated biphenyl tail gas degradation and catalytic activity recovery
Zhichao Yun1, Yuyang Bai1, Fu Xia1
1State Key Laboratory of Environmental Criteria and Risk Assessment, Chinese Research Academy of Environmental Sciences, Beijing 100012, China; State Environmental Protection Key Laboratory of Simulation and Control of Groundwater Pollution, Chinese Research Academy of Environmental Sciences, Beijing 100012, China.
Abstract:
To address the problems with catalytic degradation, such as poisoning and inactivation, a simple and efficient gas purging regeneration technique was developed for iron-based catalyst in-situ regeneration. Specifically, the effects of carrier gas types, regeneration temperatures, and granular activated carbon (GAC) addition on iron-based catalyst regeneration were investigated. The Fe3O4/γ-Al2O3 regenerated at 550 °C with additional GAC and 15 % water vapor exhibited the optimal degradation efficiency towards polychlorinated biphenyls (PCBs), with an increase from 41.2 % to 93.5 %, compared with non-regenerated Fe3O4/γ-Al2O3. In addition, the 60-hour stability test revealed a well-recovered catalytic activity. During the Fe3O4/γ-Al2O3 regeneration, the coke on the catalyst surface was oxidized and removed in the form of CO2, and meanwhile the oxidized Fe(III) was reduced into Fe(II) in the catalyst. This study provides a safe and efficient iron-based catalyst regeneration technology for PCB off-gas degradation and reveals the catalytic activity recovery mechanism during catalyst regeneration.
More Related Videos
Related Concept Videos
Bioremediation
Catalysis
Lipid Catabolism