Durability Assessment of Cement Mortars with Recycled Ceramic Powders
Anna Tokareva1, Danièle Waldmann2
1Department of Engineering, Faculty of Science, Technology and Medicine, University of Luxembourg, L-4365 Esch-sur-Alzette, Luxembourg.
Abstract:
Although substantial knowledge exists regarding the use of ceramic powders as pozzolanic supplementary cementitious materials, a notable gap remains in the literature concerning the durability properties of cement with ceramics. This research aims to address this gap by evaluating the effects of ceramic powders on mortar durability, specifically focusing on resistance to freeze-thaw, high temperatures, and 1% sulphuric acid. The study also investigates the use of recycled ceramic demolition waste as a replacement for calcined clay in limestone calcined clay (LC3) formulations. This research demonstrates the potential of using ceramic waste to enhance mortar durability. The results show significant improvements in freeze-thaw resistance, with strength losses of 1.91% to 2.61% for modified mortars, compared to 6.31% for the reference mortar. Fire resistance also improves, with strength gains of up to 13.9% at 200 °C for LC3 mortars with ceramic powder. At 500 °C, strength losses ranged from 2.8% to 31.9%, with ceramic-containing mortars showing better performance than the reference. At 900 °C, substantial strength losses occurred across all mixes (72.0% to 90.0%), with mortars containing ultrafine ceramic powder showing the best resistance. Resistance to 1% sulphuric acid is enhanced, with strength losses decreasing from 9.37% in the reference mortar to 1.38% in LC3 mortar with ceramic powder.
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Mortar Properties
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Testing Water Quality
Mortar
Porosity in Cement Paste
The balance of water to cement in the mix is...