Effects of Aged Conditions on the Self-Healing Performance of Asphalt Mixtures: A Comparative Study of Long-Term and

Zhenqing He1, Anhua Xu1, Aipeng Wang2

  • 1Key Laboratory of High Altitude and Mountain Passway Construction and Maintenance, Qinghai Vocational Technical University, Xining 810003, China.

Polymers
|October 16, 2025
PubMed

Related Concept Videos

Fatigue Strength of Concrete01:22

Fatigue Strength of Concrete

Fatigue, in the context of materials science and engineering, refers to the weakening or failure of a material caused by repeatedly applied loads, even if these loads are below the strength limit of the material. Fatigue strength in concrete is a critical property that influences its durability and longevity. Concrete can fail in two ways due to fatigue. Static fatigue or creep rupture occurs under a constant load or one that increases slowly. The other failure mode is due to cyclical or...
535
The Effect of Aging on Tissues01:19

The Effect of Aging on Tissues

Several body functions deteriorate with age. The external signs of aging are easily identifiable. For example, the skin becomes dry, less elastic, and thins out, forming wrinkles. The skin of the face begins to appear looser due to a decrease in the levels of elastic and collagen fibers in the connective tissue. Additionally, melanin production in the hair follicle decreases with age, resulting in gray hair. Moreover, the senses of sight and hearing decline, so glasses and hearing aids may...
3.3K
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
356
Hot Weather Concreting01:20

Hot Weather Concreting

Concreting at elevated temperatures accelerates the hydration process, leading to quicker setting but potentially reducing the long-term strength of the concrete structure. Additionally, low air humidity fosters rapid moisture loss from the concrete, resulting in reduced workability, pronounced plastic shrinkage, and a higher likelihood of crazing.
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
295
Effects of Air-entrainment in Concrete01:28

Effects of Air-entrainment in Concrete

Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
367
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
364