Study of multi-size proppant breakage mechanism under deep reservoir conditions for enhanced geothermal system

Buge Du1, Guangqing Zhang2,3, Ruiheng Jin1

  • 1Department of Petroleum Engineering, China University of Petroleum-Beijing, Beijing, 102249, China.

Scientific Reports
|October 24, 2025
PubMed

Related Concept Videos

Pore Size Distribution01:23

Pore Size Distribution

In concrete, the pore size distribution significantly influences the material's properties. Capillary pores, markedly larger than gel pores, form a vast network within partially hydrated cement paste, reducing the concrete's strength and increasing its permeability. This heightened permeability leads to a greater risk of damage from environmental factors like freeze-thaw cycles and chemical attacks, with the extent of vulnerability also being tied to the water-to-cement ratio.
Adequate...
433
Porosity and Absorption of Aggregate01:20

Porosity and Absorption of Aggregate

Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
735
Typical Model Studies01:30

Typical Model Studies

Fluid mechanics model studies often utilize scaled-down systems to predict fluid behavior in full-scale environments, such as river flows, dam spillways, and structures interacting with open surfaces. Maintaining Froude number similarity in river models is crucial, as it replicates surface flow features like wave patterns and velocities.
616
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
431