Low-Temperature Performance Enhancement of Warm Mix Asphalt Binders Using SBS and Sasobit: Towards Durable and Green

Xuemao Feng1,2, Mingchen Li3, Yifu Meng4

  • 1Guangxi New Development Transportation Group Co., Nanning 530029, China.

PubMed

Related Concept Videos

Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
294
Hot Weather Concreting01:20

Hot Weather Concreting

Concreting at elevated temperatures accelerates the hydration process, leading to quicker setting but potentially reducing the long-term strength of the concrete structure. Additionally, low air humidity fosters rapid moisture loss from the concrete, resulting in reduced workability, pronounced plastic shrinkage, and a higher likelihood of crazing.
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
293
Superplasticizers01:30

Superplasticizers

Superplasticizers are advanced admixtures that enhance the workability of concrete by lowering the water content without compromising the strength of the material. These substances are highly effective water reducers, improving concrete flow, making it easier to work with, and enabling concrete to reach inaccessible areas or densely reinforced sections without mechanical vibration. The key components in superplasticizers are either sulfonated melamine or naphthalene formaldehyde condensates,...
301
Cold Weather Concreting01:27

Cold Weather Concreting

When freshly poured concrete is exposed to freezing temperatures before it has set, the water within the concrete can freeze. This expansion disrupts the setting process, delays chemical reactions necessary for hardening, and increases the volume of pores within the hardened concrete, which weakens its overall structure. If the concrete manages to reach an appreciable strength before it freezes, the damage can be somewhat mitigated.
To counteract the negative impacts of cold weather, ensuring...
350
Accelerators01:17

Accelerators

Accelerators in concrete serve as admixtures to speed up the hardening process, enabling the concrete to achieve early strength faster. Although accelerators do not necessarily impact the time it takes concrete to set, they reduce this time in practice. A common accelerator is calcium chloride, which is particularly useful for hastening early strength development in cold weather or for rapid repair jobs that require quick heat generation after mixing.
The effectiveness of calcium chloride can...
265
Waterproofing and Anti-Bacterial Admixtures in Concrete01:22

Waterproofing and Anti-Bacterial Admixtures in Concrete

Concrete's susceptibility to water absorption is due to the capillary action within the pores of its hydrated cement paste. This action draws water in, creating the need for waterproofing admixtures to prevent such penetration. The efficacy of these admixtures is contingent upon the water pressure, with variations arising from different conditions such as rain, capillary rise, or hydrostatic pressure in structures intended to hold water.
Waterproofing admixtures render concrete hydrophobic,...
221