Experimental Verification of Calcite Formation Potential by Ureolytic and Non-Ureolytic Bacterial Strains in

Bashar Al Hayo1, Orhan Canpolat1, Nihal Doğruöz Güngör2

  • 1Department of Civil Engineering, Faculty of Civil Engineering, Yildiz Technical University, İstanbul 34220, Türkiye.

PubMed

Related Concept Videos

Hydration of Cement01:24

Hydration of Cement

Hydration of cement is a chemical reaction between cement particles and water. This process occurs primarily through two mechanisms: through-solution and topochemical. In the through-solution process, anhydrous compounds dissolve into their constituents, hydrates form in the solution, and then precipitate from the supersaturated solution. The topochemical process involves solid-state reactions at the cement particle surface. The through-solution process dominates the topochemical process at the...
797
Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...
461
Mortar Properties01:17

Mortar Properties

Mortar properties encompass a range of characteristics crucial for construction and masonry work, including workability, water retention, bond strength, durability, compressive strength, volume change, and appearance. Workability refers to mortar's ability to be easily applied and manipulated without sagging or falling off surfaces, which is important for efficient masonry unit placement and alignment. Water retention is essential to prevent the mortar from losing moisture too quickly to...
422
Soundness of Cement01:17

Soundness of Cement

The soundness of cement refers to the ability of cement paste to retain its volume after setting. Unsound cement can lead to expansion and structural damage due to the presence of free lime, magnesia, and calcium sulfate. Free lime hydrates very slowly, expanding and causing unsoundness, which is difficult to detect because it intercrystallizes with other compounds. Magnesia also reacts with water, forming crystals that can disrupt the cement's structure. Calcium sulfate can create...
511
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
448
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
346