Data-Driven Fatigue Prediction of Superalloys: A Novel Strategy Integrating Transfer Learning and Partial Label

Haopeng Lv1, Jiawei Yin1, Dayong Wu1,2

  • 1School of Materials Science and Engineering, Hebei University of Science and Technology, Shijiazhuang, Hebei, 050018, P. R. China.