Area-Selective Low-Pressure Thermal Atomic Layer Deposition of Gallium Nitride
Bernhard Y van der Wel1, Kees van der Zouw1, Antonius A I Aarnink1
1MESA+ Institute for Nanotechnology, University of Twente, P.O. Box 217, Enschede 7500 AE, The Netherlands.
Abstract:
This work reports on the successful intrinsic area-selective deposition of GaN films by thermal atomic layer deposition at back-end-of-line compatible temperatures. Using sequential pulses of trimethylgallium and ammonia (NH3) at a substrate temperature of 673 K, polycrystalline GaN is selectively formed onto AlN on substrates consisting of patterned AlN on thermal SiO2. Before the deposition of GaN, a thin film of AlN is deposited selectively by atomic layer deposition on the patterned AlN to enable the deposition of GaN on AlN. The interfaces and layer thicknesses were examined by transmission electron microscopy, spectroscopic ellipsometry, and atomic force microscopy.
More Related Videos
14:16Fabrication of Schottky Diodes on Zn-polar BeMgZnO/ZnO Heterostructure Grown by Plasma-assisted Molecular Beam Epitaxy
Published on: October 23, 2018
07:00Graphene-Assisted Quasi-van der Waals Epitaxy of AlN Film on Nano-Patterned Sapphire Substrate for Ultraviolet Light Emitting Diodes
Published on: June 25, 2020
Related Concept Videos
Nuclear Fission
Nuclear Power
Nuclear Fuels
Nuclear fuel consists of a fissile isotope, such as uranium-235, which must be present in sufficient quantity to provide a...
Nuclear Transmutation
Atomic Absorption Spectroscopy: Atomization Methods
Atomic Absorption Spectroscopy: Lab
Solutions containing organic solvents, such as low-molecular-mass alcohols, esters, or ketones, enhance absorbances by increasing nebulizer...