Dynamic behavior and micro-meso scale fracture mechanisms of sandstone under long-term water immersion

Xiaowei Gu1,2,3, Chujian Han1,2,3, Xiaochuan Xu1,2,3

  • 1School of Resources and Civil Engineering, Northeastern University, Shenyang, 110819, China.

Scientific Reports
|December 14, 2025
PubMed

Related Concept Videos

Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
404
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
332
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
313
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
932
Behavior of Concrete Under Compressive Load01:23

Behavior of Concrete Under Compressive Load

Concrete exhibits specific behaviors under different compressive loads. Understanding this is crucial for understanding its structural integrity. When concrete undergoes uniaxial compression, it tends to develop cracks that run parallel to the direction of the force. These parallel cracks stem from localized tensile stresses that occur perpendicular to the compression direction. Additionally, angled cracks may appear due to the formation of shear planes.
As the concrete specimen fractures under...
544
Creep in Concrete01:22

Creep in Concrete

Creep refers to the time-dependent increase in strain under a sustained load, excluding other time-dependent deformations associated with shrinkage, swelling, and thermal expansion in concrete. The primary mechanism behind creep involves the loss of physically adsorbed water from the calcium silicate hydrate within the hydrated cement paste. This process is further exacerbated by concrete's non-linear stress-strain relationship, microcrack development in the interfacial transition zone, and...
1.1K