Hot Deformation Behavior via Isothermal Compression and Constitutive Model of GH2132 Superalloy

Yue Sun1,2, Peng Cheng1, Decheng Wang1,2

  • 1China Productivity Center for Machinery, China Academy of Machinery Science and Technology, Beijing 100044, China.

PubMed

Related Concept Videos

Temperature Dependent Deformation01:12

Temperature Dependent Deformation

In a nonhomogeneous rod made up of steel and brass, restrained at both ends and subjected to a temperature change, several steps are involved in calculating the stress and compressive load. Due to the problem's static indeterminacy, one end support is disconnected, allowing the rod to experience the temperature change freely. Next, an unknown force is applied at the free end, triggering deformations in the rod's steel and brass portions. These deformations are then calculated and added...
343
Stress-Strain Diagram - Ductile Materials01:24

Stress-Strain Diagram - Ductile Materials

The stress-strain relationship in ductile materials such as structural steel or aluminium is intricate and progresses through several stages. When a specimen is loaded, it initially exhibits a linear length increase, depicted by a steep straight line on the stress-strain diagram. It indicates the material is elastically deforming and will return to its original shape once unloaded. However, when a critical stress value is reached, plastic deformation begins. This stage sees substantial...
1.8K
Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
494
Yield Criteria for Ductile Materials under Plane Stress01:25

Yield Criteria for Ductile Materials under Plane Stress

In designing structural elements and machine parts using ductile materials, it is crucial to ensure that these components withstand applied stresses without yielding. Yielding is initially determined through a tensile test, which evaluates the material's response to uniaxial stress. However, tensile stress is insufficient when components face biaxial or plane stress conditions This condition requires advanced criteria to predict failure.
The Maximum Shearing Stress Criterion, also known as...
448
Mechanical Characteristics of Steel01:18

Mechanical Characteristics of Steel

The mechanical characteristics of steel are assessed through various tests that evaluate its strength, toughness, and flexibility. These tests include tension, torsion, impact, bending, and hardness assessments, each providing crucial information about steel's suitability for specific applications.
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
989
Hooke's Law01:26

Hooke's Law

Hooke's law, a pivotal principle in material science, establishes that the strain a material undergoes is directly proportional to the applied stress, defined by a factor called the modulus of elasticity or Young's modulus.
1.4K