An Atomistic Investigation of Cobalt's Nanoindentation Response with An Angular Dependent Potential

Douglas S Oliveira1, Danilo P Kuritza1, José E Padilha1

  • 1Universidade Federal do Paraná, Campus Avançado de Jandaia do Sul, 86900-000 Jandaia do Sul, Paraná, Brazil.

ACS Omega
|February 9, 2026
PubMed

Related Concept Videos

Van der Waals Interactions01:24

Van der Waals Interactions

Atoms and molecules interact with each other through intermolecular forces. These electrostatic forces arise from attractive or repulsive interactions between particles with permanent, partial, or temporary charges. The intermolecular forces between neutral atoms and molecules are ion–dipole, dipole–dipole, and dispersion forces, collectively known as van der Waals forces.
Bonding in Metals02:32

Bonding in Metals

Metallic bonds are formed between two metal atoms. A simplified model to describe metallic bonding has been developed by Paul Drüde called the “Electron Sea Model”.
Valence Bond Theory02:42

Valence Bond Theory

Coordination compounds and complexes exhibit different colors, geometries, and magnetic behavior, depending on the metal atom/ion and ligands from which they are composed. In an attempt to explain the bonding and structure of coordination complexes, Linus Pauling proposed the valence bond theory, or VBT, using the concepts of hybridization and the overlapping of the atomic orbitals. According to VBT, the central metal atom or ion (Lewis acid) hybridizes to provide empty orbitals of suitable...
Crystal Field Theory - Octahedral Complexes02:58

Crystal Field Theory - Octahedral Complexes

Crystal Field Theory
To explain the observed behavior of transition metal complexes (such as colors), a model involving electrostatic interactions between the electrons from the ligands and the electrons in the unhybridized d orbitals of the central metal atom has been developed. This electrostatic model is crystal field theory (CFT). It helps to understand, interpret, and predict the colors, magnetic behavior, and some structures of coordination compounds of transition metals.
CFT focuses on...
Angular Momentum: Single Particle01:10

Angular Momentum: Single Particle

Angular momentum is directed perpendicular to the plane of the rotation, and its magnitude depends on the choice of the origin. The perpendicular vector joining the linear momentum vector of an object to the origin is called the “lever arm.” If the lever arm and linear momentum are collinear, then the magnitude of the angular momentum is zero. Therefore, in this case, the object rotates about the origin such that it lies on the rim of the circumference defined by the lever arm magnitude.
The...
Atomic Force Microscopy01:08

Atomic Force Microscopy

Atomic force microscopy (AFM) is a type of scanning probe microscopy that can analyze topographic details of various specimens like ceramics, glass, polymers, and biological samples. AFM offers over 1000 times more resolution than the optical imaging system. Images generated from AFM are three-dimensional surface profiles, offering an advantage over the flat, two-dimensional images from other imaging techniques.
The AFM Probe
The probe is regarded as the heart of any AFM setup and comprises the...