Study on the Morphological Distribution and Formation Mechanisms of Residual Polymer in Polymer-Containing Wastewater
Zengbao Wang1,2, Junjie Jiang1, HongJian Ni1
1School of Petroleum Engineering, China University of Petroleum (East China), Qingdao 266580, China.
Abstract:
Polymer flooding is a crucial enhanced oil recovery (EOR) technique; however, postpolymer flooding, reinjected polymer-laden wastewater tends to trigger filter clogging and near-wellbore region permeability damage due to colloidal aggregation. This study investigates the microscopic morphological characteristics, aggregation mechanisms, and dominant factors of residual polymers through multiscale experiments. The basic properties, dispersion morphology, and stability of residual polymers in produced water were characterized by using iodine-starch colorimetry, scanning electron microscopy (SEM), zeta potential analysis, and dynamic light scattering (DLS). The effects of Na+, Ca2+, Fe3+, and clay on polymer morphology, size, and stability were systematically explored. Results indicate that the molecular weight of residual polymers in produced water decreases by ∼90% compared to preinjection polymers, accompanied by a significant viscosity reduction. Microstructurally, the polymer transitions from linear long-chain configurations to colloidal clusters exhibiting "deep-ravine" or flocculent structures. The zeta potential (0-10 mV) confirms the system's high instability, rendering it prone to rapid aggregation and blockage. Na+ induces molecular chain coiling through charge screening effects, while Ca2+ intensifies compression and dehydration processes, resulting in polymer molecular aggregation. Fe3+ triggers cross-linked flocculation via charge neutralization and bridging mechanisms. Concurrently, clay minerals adsorb polymer fragments to form encapsulating structures, expanding particle diameters by 3.8-6.8 times and significantly compromising system stability. Formation shear further fractures polymer chains, while synergistic interactions between clay and Fe3+ (amplifying particle sizes by 6.8 and 2.5×) dominate flocculation, the paramount cause of plugging. This study provides theoretical guidance for optimizing polymer-containing wastewater treatment processes and developing anticlogging technologies.
Related Concept Videos
Polymer Classification: Architecture
Polymers
Step-Growth Polymerization: Overview
Many natural and synthetic polymers are produced by...
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...