Solvent-Based Separation of PA6 and PET Using Solubility Data from Differential Scanning Calorimetry
Ruben Goldhahn1, Ann-Joelle Minor2, Liisa Rihko-Struckmann1
1Department of Process Systems Engineering, Max Planck Institute for Dynamics of Complex Technical Systems, Sandtorstraße 1, Magdeburg 39106, Germany.
None:
To minimize plastic pollution and prevent further extraction of fossil feedstock, the circular economy for polymers offers a promising solution. As an integral part of the circular economy to close material loops, solvent-based recycling enables the separation of mixed plastic waste into pure component streams without altering the polymer structure but requires reliable solubility data of polymers in solvents. We present a standardized differential scanning calorimetry (DSC) protocol to determine decrystallization and precipitation temperatures of polymers in various solvents and apply it to the challenging separation of polyamide 6 (PA6) and polyethylene terephthalate (PET). The DSC method enables quantitative solubility analysis even above solvent boiling points and shows good agreement with a visual polythermal cloud point method while offering higher objectivity and additional phase transition enthalpies. Temperature-dependent solubility data for nine solvents reveal that methanol, ethanol, propylene glycol, dimethyl sulfoxide, and water are selective solvents for PA6 over PET. A proof-of-concept PA6-PET separation using methanol yields recycled polymers with near-virgin properties under mild conditions (109 °C, ∼4 bar), demonstrating the process relevance of the obtained DSC data for solvent selection in low-energy, solvent-based recycling processes.
More Related Videos
10:22Designed for Molecular Recycling: A Lignin-Derived Semi-aromatic Biobased Polymer
Published on: November 30, 2020
05:05Quantification of Polybutylene Adipate Terephthalate-based Micro- and Nano-plastics from Soil Using Proton Nuclear Magnetic Resonance Spectroscopy
Published on: June 6, 2025