Abstract:
Shop-floor weld inspection may appear to be a solved problem until a camera is deployed near a galvanized-sheet MIG welding line. The seam reflects light, the texture changes from frame to frame, and the defects of interest are often small and visually subtle. Additionally, the hardware near the line is rarely a data-center GPU. With those constraints in mind, this paper presents YOLO-MIG, a compact detector built on YOLOv10n for weld-seam inspection in practical production conditions. We make three focused changes to the baseline: a C2f-EMSCP backbone block to better preserve weak defect cues with modest parameter growth, a BiFPN neck to keep small-target information alive during feature fusion, and a C2fCIB head to clean up predictions that otherwise get distracted by seam edges and illumination artifacts. On a workshop-collected dataset containing 326 original images, with the training subset expanded through augmentation to 2608 labeled samples in total, YOLO-MIG achieves 98.4% mAP@0.5 and 56.29% mAP@0.5:0.95 on the test set while remaining lightweight (1.83 M parameters, 3.87 MB FP16 weights). Compared with YOLOv10n, the proposed model improves mAP@0.5 by 9.36 points and mAP@0.5:0.95 by 4.89 points, while reducing parameters, GFLOPs, and model size by 43.4%, 19.9%, and 29.9%, respectively. The results suggest that YOLO-MIG is not only accurate but also realistic to deploy at the edge for intelligent weld quality control.
Related Concept Videos
Lumber Defects
Shakes are minor fractures that run along or across the wood's annual rings, while wane is...
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Steel Manufacturing
During this smelting process, limestone plays a crucial role by forming slag. Slag captures impurities within the molten iron, such...
Structural Steel Products
Once shaped, the steel's final form emerges as a continuous length, which is then segmented by a hot saw into manageable pieces. These segments...
Steel Fastening Techniques
Rivets are cylindrical steel fasteners with a specially designed head. During application, rivets are heated until white-hot and then inserted through pre-drilled holes in the steel sections. A pneumatic hammer is used to shape the exposed end into a second head, securing the sections together.
Bolting is another...
Unsymmetric Loading of Thin-Walled Members: Problem Solving
To compute the shear forces, find the shear flow at a specific distance from the endpoint using the vertical shear and the moment of inertia values. The total shear force on the flange is calculated by integrating the shear flow from one end of the flange to the other.
Next, calculate the moments of...