Abstract:
Electrochemical energy storage devices commonly face a trade-off between specific energy and power capability. Black phosphorus offers a high theoretical capacity of 2596 mA h g-1, but its practical application is limited by slow reaction kinetics during multiphase phosphorus redox processes. These sluggish transformations, involving bond rearrangement and soluble intermediates, hinder fast charging and compromise cycling stability. Here we show that introducing phosphorus-nitrogen bonds into a black phosphorus/carbon composite regulates the reaction pathway and accelerates charge transport. The engineered bonding environment modifies the electronic structure of black phosphorus and lowers lithium-ion diffusion barriers, enabling faster lithiation and delithiation. Meanwhile, nitrogen sites in the carbon matrix confine lithium-phosphorus intermediates, reducing their migration and improving structural stability. This combined effect enhances both rate capability and reversibility. When coupled with lithium iron phosphate in a pouch cell, the composite negative electrode delivers a specific energy of 282 Wh kg-1 and retains 80% of its capacity after 10 min of charging at high specific current. The device also maintains stable operation over thousands of cycles, demonstrating improved durability under fast charging conditions.
More Related Videos
07:55Elemental-sensitive Detection of the Chemistry in Batteries through Soft X-ray Absorption Spectroscopy and Resonant Inelastic X-ray Scattering
Published on: April 17, 2018
10:03Characterization of Electrode Materials for Lithium Ion and Sodium Ion Batteries Using Synchrotron Radiation Techniques
Published on: November 11, 2013
Related Concept Videos
The Electrical Double Layer
Ladder Diagrams: Redox Equilibria
Consider the Fe3+/Fe2+ half-reaction, which has a standard-state potential of +0.771 V. At potentials more positive than +0.771 V, Fe3+ predominates, whereas Fe2+...
Biasing of P-N Junction
In equilibrium, no external voltage is applied across the p-n junction. The depletion region is formed at the junction interface due to the diffusion of carriers, which leaves behind charged dopants, acceptors on the p-side, and donors on the n-side. These immobile charges create an electric field that prevents further diffusion of carriers. The related energy band...