Prediction of Bond Strength in Corroded Reinforced Concrete Using SVM and XGB Methods

Zhi-Qiang Chen1,2,3, Zhuang Chen1, Ying-Zi Zhong1

  • 1School of Architecture and Civil Engineering, Chengdu University, Chengdu 610106, China.

Abstract

Related Concept Videos

Bonding and Strength of Aggregate01:12

Bonding and Strength of Aggregate

The bond between aggregate particles and the cement matrix is significantly influenced by the shape and surface texture of the aggregates. High-strength concretes benefit from a rougher texture, which leads to stronger bonding due to greater adhesion. Angular aggregates with larger surface areas also enhance this bond. The bonding quality, however, is complex to assess as no universally accepted test exists. Good bonding is indicated when a crushed concrete specimen shows some aggregate...
Non-destructive Tests for Concrete Strength01:12

Non-destructive Tests for Concrete Strength

The rebound hammer test, also known as the Schmidt hammer test, is a non-destructive technique for evaluating the hardness of concrete and, indirectly, the strength of concrete. It operates on the principle that the rebound of a spring-driven mass from a concrete surface correlates to the surface's hardness. The device comprises a mass within a tubular housing, a spring mechanism, and a plunger that strikes the concrete. Upon release, the energy imparted to the mass by the spring causes it to...
Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Abrasion Resistance of Concrete01:23

Abrasion Resistance of Concrete

Abrasion resistance is an essential characteristic of concrete that determines its durability and longevity under various wear conditions. Concrete surfaces are vulnerable to different types of abrasion. For instance, surfaces may wear down due to the constant movement of vehicles or be eroded by solids carried in water, as seen in concrete canal linings. Specific tests are conducted to measure the abrasion resistance of concrete.
One such test is the revolving disc test, where three plates...
Sulfate Attack on Concrete01:29

Sulfate Attack on Concrete

Sulfate attack on concrete is a deterioration process characterized by a whitish discoloration beginning at the edges and corners, accompanied by cracking and spalling. This phenomenon occurs when sulfates react with the components of hardened concrete, forming compounds like calcium sulfate and calcium sulfoaluminate which occupy more space than the substances they replace, causing the concrete to expand and disrupt.
Sulfates from sources like soil, groundwater, or industrial effluents...