The Effects of Long-Term High-Temperature Aging on the Microstructural Evolution and Impact Fracture Behavior of

Zhining Li1, Kejian Li1, Yao Wu1

  • 1Department of Mechanical Engineering, Tsinghua University, Beijing 100084, China.

Related Concept Videos

Effects of Creep01:25

Effects of Creep

Creep in concrete, the gradual deformation under prolonged stress, significantly impacts the integrity of structures. For reinforced concrete beams, it can be a vital design consideration, as it increases deflection, sometimes necessitating additional design measures. In columns, especially slender ones under eccentric loads, creep can cause buckling, compromising their stability. However, creep can be beneficial in indeterminate structures by mitigating stresses that arise from shrinkage,...
Fatigue01:21

Fatigue

Fatigue occurs when materials rupture under repeated or fluctuating loads, even at stress levels far below their static breaking strength. It typically results in brittle failure, even for ductile materials. It is a critical consideration in designing machines and structural components subjected to repetitive or varying loads. The nature of these loadings can range from fluctuating loads like unbalanced pump impellers causing vibrations to repeatedly bending a thin steel rod wire back and forth...
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
Temperature Dependent Deformation01:12

Temperature Dependent Deformation

In a nonhomogeneous rod made up of steel and brass, restrained at both ends and subjected to a temperature change, several steps are involved in calculating the stress and compressive load. Due to the problem's static indeterminacy, one end support is disconnected, allowing the rod to experience the temperature change freely. Next, an unknown force is applied at the free end, triggering deformations in the rod's steel and brass portions. These deformations are then calculated and added together...
Thermal Strain01:19

Thermal Strain

Thermal strain is a concept that arises when we consider how temperature changes affect structures. Unlike the conventional assumption that structures remain constant under load, real-world scenarios often involve temperature fluctuations that can significantly impact these structures. Consider a homogeneous rod with a uniform cross-section resting freely on a flat horizontal surface. If the rod's temperature increases, the rod elongates. This elongation is proportional to the temperature...
Residual Stresses01:26

Residual Stresses

Residual stresses reside in a structure even after removing the original stress inducer. This phenomenon often arises from varied plastic deformations across different parts of a structure. Consider a rod stretched beyond its yield point. It will not regain its original length due to permanent deformation. Even after load removal, the rod does not entirely lose stress because of uneven plastic deformations, resulting in residual stresses. The computation of these stresses in structures is...