Effects of Warm-Mix Agents on the Thermal Stability of SBS-Modified Asphalt

Qingdong Tao1, Tianhong Xia1, Desheng Yang2

  • 1School of Architectural Engineering, Mianyang Polytechnic, Mianyang 621000, China.

Related Concept Videos

Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
To address...
Hot Weather Concreting01:20

Hot Weather Concreting

Concreting at elevated temperatures accelerates the hydration process, leading to quicker setting but potentially reducing the long-term strength of the concrete structure. Additionally, low air humidity fosters rapid moisture loss from the concrete, resulting in reduced workability, pronounced plastic shrinkage, and a higher likelihood of crazing.
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
Masonry in Cold and Hot Weather Conditions01:21

Masonry in Cold and Hot Weather Conditions

In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units and sand dry and...
Effects of Air-entrainment in Concrete01:28

Effects of Air-entrainment in Concrete

Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
Cold Weather Concreting01:27

Cold Weather Concreting

When freshly poured concrete is exposed to freezing temperatures before it has set, the water within the concrete can freeze. This expansion disrupts the setting process, delays chemical reactions necessary for hardening, and increases the volume of pores within the hardened concrete, which weakens its overall structure. If the concrete manages to reach an appreciable strength before it freezes, the damage can be somewhat mitigated.
To counteract the negative impacts of cold weather, ensuring...
Retarders01:19

Retarders

Retarders are chemical admixtures designed to extend the setting time, which is especially useful when there is a delay in sequential concrete pours to prevent cold joints and to achieve a cohesive structure. Retarders, when used in appropriate amounts, can also enhance the architectural appearance of exposed aggregate finishes.