Novel core-shell structured Fe@Al2O3 nanofibers prepared by atomic layer deposition as a high-performance microwave

Xiaoqiang Li1, Jun Xiang2, Jinnan Yang2

  • 1College of Physics and Electronic Engineering, Xinyang Normal University, Xinyang, 464300, China. lxqxynu@163.com.