Physico-chemical analysis of eight pre-mixed hydraulic silicate sealers

Vasileios Kapralos1, Matthias Zehnder1

  • 1Clinic for Conservative and Preventive Dentistry, Center for Dental Medicine, University of Zurich, Zurich, Switzerland.

Abstract

Related Concept Videos

Hydration of Cement01:24

Hydration of Cement

Hydration of cement is a chemical reaction between cement particles and water. This process occurs primarily through two mechanisms: through-solution and topochemical. In the through-solution process, anhydrous compounds dissolve into their constituents, hydrates form in the solution, and then precipitate from the supersaturated solution. The topochemical process involves solid-state reactions at the cement particle surface. The through-solution process dominates the topochemical process at the...
Plasticizers01:31

Plasticizers

Water-reducers, or plasticizers, are chemical admixtures used in concrete to improve strength and workability. These additives reduce the water-cement ratio without compromising workability, lower the cement content while maintaining the same workability, or increase workability to assist concrete placement in inaccessible areas.
Plasticizers function by using surface-active agents to create repulsive electrostatic forces between cement particles. This dispersion enhances the concrete's...
Waterproofing and Anti-Bacterial Admixtures in Concrete01:22

Waterproofing and Anti-Bacterial Admixtures in Concrete

Concrete's susceptibility to water absorption is due to the capillary action within the pores of its hydrated cement paste. This action draws water in, creating the need for waterproofing admixtures to prevent such penetration. The efficacy of these admixtures is contingent upon the water pressure, with variations arising from different conditions such as rain, capillary rise, or hydrostatic pressure in structures intended to hold water.
Waterproofing admixtures render concrete hydrophobic,...
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
Superplasticizers01:30

Superplasticizers

Superplasticizers are advanced admixtures that enhance the workability of concrete by lowering the water content without compromising the strength of the material. These substances are highly effective water reducers, improving concrete flow, making it easier to work with, and enabling concrete to reach inaccessible areas or densely reinforced sections without mechanical vibration. The key components in superplasticizers are either sulfonated melamine or naphthalene formaldehyde condensates,...
Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...