Effects of Mineral Raw Materials on Melting-Crystallization Properties and Microstructure of Fluorine-Free Mold Flux
Di Zhang1,2, Xiuli Han1,2, Lei Liu1,2
1College of Mining Engineering, North China University of Science and Technology, Tangshan 063210, China.
Abstract:
During the continuous casting of high-titanium steel, traditional fluorine-containing mold fluxes are prone to causing fluoride contamination, equipment corrosion, and intensified slag-metal interface reactions. There is an urgent need to develop highly adaptable fluorine-free mold flux systems. In this study, titanium-containing blast furnace slag was used as the primary base material, while borax, soda ash, and witherite were selected as fluoride-substituting mineral raw materials. The effects of these mineral raw materials on the melting properties, crystallization behavior, crystalline phases, and microstructure of fluorine-free mold fluxes were systematically investigated, and an optimized mold flux design suitable for continuous casting of high-titanium steel was further developed. The results indicate that borax significantly reduces the melting temperature and viscosity and markedly suppresses the growth of crystalline phases such as calcium borosilicate, nepheline, and perovskite by weakening the polymerization degree of the silicate network, thereby substantially decreasing the crystallization ability of the mold flux. Soda ash primarily acts as a strong fluxing and network-depolymerizing agent, promoting the formation of low-polymerized structural units. It also enhances the tendency toward ordered atomic arrangement, thereby markedly increasing nepheline precipitation and the overall crystallization ratio. Witherite exerts a relatively mild effect on slag structure and phase evolution; its moderate addition helps synergistically reduce the melting point, viscosity, and crystallization ratio, thereby supporting performance stability. The optimized fluorine-free mold flux, designed on the basis of these findings, maintains a suitable initial crystallization temperature and critical crystallization cooling rate while exhibiting lower melting temperature, viscosity, and crystallization ratio than conventional fluorine-bearing flux. The findings establish a theoretical basis for designing eco-friendly mold fluxes suitable for high-titanium steel and for enhancing billet quality.
Related Concept Videos
Steel Manufacturing
During this smelting process, limestone plays a crucial role by forming slag. Slag captures impurities within the molten iron, such...
Sample Preparation for Analysis: Advanced Techniques
Acid digestion with strong acids is commonly used to dissolve inorganic materials that are insoluble (do not dissolve) in water. This method can be useful for...