Related Experiment Video
Updated: Jun 27, 2026

Mechanical Expansion of Steel Tubing as a Solution to Leaky Wellbores
Published on: November 20, 2014
Mechanical Behavior and Damage Characteristics of Cemented Tailings Backfill Under Multiple Different Stress
Xiaofei Li1,2, Yuanfan Liu1, Jie Wang1
1School of Resources and Safety Engineering, University of Science and Technology Beijing, Beijing 100083, China.
Abstract:
To investigate the impact of underground multiple stress disturbances on the long-term stability of cemented tailings backfill (CTB), this study conducted experiments under different disturbance levels (20-80% of static strength) and frequencies (1-4 times). By comprehensively utilizing mechanical testing, wave velocity monitoring, digital image correlation (DIC), and scanning electron microscopy (SEM), the "heterogeneous" evolution mechanism of macro-micro damage was revealed. The results indicate that disturbance level and frequency exert distinctly different driving effects on the deterioration of CTB, rather than a simple linear superposition. Specifically, low-frequency disturbance produces a compaction strengthening effect, microscopically promoting the generation of Ca(OH)2 and ettringite (increased Ca/Si ratio). In contrast, the combination of high disturbance and high frequency induces free water extrusion and inhibits hydration, leading to an advanced damage threshold based on energy evolution and the accelerated coalescence of microcracks, which favors the formation of C-S-H gel (decreased Ca/Si ratio). Within this heterogeneous mechanism, the disturbance level acts as the dominant controlling factor. This study clarifies the nonlinear mechanical and chemical evolution paths under composite disturbances, providing theoretical support for the dynamic stability control of backfill in deep multi-step mining.
More Related Videos
Related Concept Videos
Behavior of Concrete Under Compressive Load
As the concrete specimen fractures under...
Soundness of Cement
Fatigue
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...
Stresses under Combined Loadings
The process begins by slicing the tube at critical points and analyzing the internal forces and stress components at these sections, focusing on the centroid. Normal stresses, generated by axial forces and bending moments, are either compressive or tensile and vary across the section from...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...