Jove
Visualize
Contact Us
JoVE
x logofacebook logolinkedin logoyoutube logo
ABOUT JoVE
OverviewLeadershipBlogJoVE Help Center
AUTHORS
Publishing ProcessEditorial BoardScope & PoliciesPeer ReviewFAQSubmit
LIBRARIANS
TestimonialsSubscriptionsAccessResourcesLibrary Advisory BoardFAQ
RESEARCH
JoVE JournalMethods CollectionsJoVE Encyclopedia of ExperimentsArchive
EDUCATION
JoVE CoreJoVE BusinessJoVE Science EducationJoVE Lab ManualFaculty Resource CenterFaculty Site
Terms & Conditions of Use
Privacy Policy
Policies

Related Concept Videos

You might also read

Related Articles

Articles linked to this work by shared authors, journal, and citation graph.

Sort by
Same author

Countering the Faltering Ability of Warming Oceans to Absorb CO<sub>2</sub> by Adding Silica and Other Nanoparticles.

Environmental science & technology·2026
Same author

Review on band structure and spin polarization of altermagnetic materials.

Reports on progress in physics. Physical Society (Great Britain)·2026
Same author

Achieving Fermi-Level Depinning and Ideal Metal Contact in <i>β</i>-Ga<sub>2</sub>O<sub>3</sub> Devices via MXene Integration.

Nano letters·2026
Same author

An integrated framework TSV-INet for arbitrarily distributed TSV interposer wafer warpage simulation.

Microsystems & nanoengineering·2026
Same author

A unified viscoelastic-viscoplastic constitutive framework for optically clear adhesives: Experiments, modeling, and FE validation.

Microsystems & nanoengineering·2026
Same author

Artificial intelligence for detecting fetal orofacial clefts and advancing medical education.

Nature communications·2026

Related Experiment Video

Updated: Jul 8, 2026

Atomically Traceable Nanostructure Fabrication
12:35

Atomically Traceable Nanostructure Fabrication

Published on: July 17, 2015

Simulation-Guided Atomic Layer Deposition Enables Deterministic Interfacial Mechanics for Predictive Nanoimprint

Chaoyu Chen1,2,3, Jiulong Li1,2,3, Youquan Jiang1,2,3

  • 1School of Integrated Circuits, Wuhan University, Wuhan, Hubei 430072, China.

ACS Applied Materials & Interfaces
|July 7, 2026
PubMed
Summary

Molecular/atomic layer deposition (MLD/ALD) coatings improve nanoimprint lithography (NIL) by controlling mold-resist interface interactions. Graphene coatings significantly reduce stress and deformation, enabling scalable nanomanufacturing.

Keywords:
ALD/MLD coatingsinterfacial mechanicsnanoimprint lithographypattern transferpredictive framework

More Related Videos

Large-area Scanning Probe Nanolithography Facilitated by Automated Alignment and Its Application to Substrate Fabrication for Cell Culture Studies
09:45

Large-area Scanning Probe Nanolithography Facilitated by Automated Alignment and Its Application to Substrate Fabrication for Cell Culture Studies

Published on: June 12, 2018

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films
08:49

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films

Published on: December 4, 2014

Related Experiment Videos

Last Updated: Jul 8, 2026

Atomically Traceable Nanostructure Fabrication
12:35

Atomically Traceable Nanostructure Fabrication

Published on: July 17, 2015

Large-area Scanning Probe Nanolithography Facilitated by Automated Alignment and Its Application to Substrate Fabrication for Cell Culture Studies
09:45

Large-area Scanning Probe Nanolithography Facilitated by Automated Alignment and Its Application to Substrate Fabrication for Cell Culture Studies

Published on: June 12, 2018

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films
08:49

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films

Published on: December 4, 2014

Area of Science:

  • Materials Science
  • Nanotechnology
  • Manufacturing Engineering

Background:

  • Nanoimprint lithography (NIL) faces scalability challenges due to mold-resist interface issues like fracture and deformation.
  • Current NIL methods lack coordinated control over adhesion, friction, and stress during imprinting.

Purpose of the Study:

  • To develop a strategy for actively regulating interfacial interactions in NIL using conformal molecular/atomic layer deposition (MLD/ALD) coatings.
  • To investigate graphene, Al2O3, and polyurea as MLD/ALD-grown interfacial layers for NIL molds.

Main Methods:

  • Integrated molecular dynamics simulations, finite element modeling, atomic force microscopy (AFM), and experimental imprinting.
  • Systematic investigation of MLD/ALD-grown materials (graphene, Al2O3, polyurea) as NIL mold interfacial layers.

Main Results:

  • Established quantitative links between coating chemistry, interfacial energetics, stress evolution, and pattern fidelity.
  • Graphene coatings reduced imprint-induced mechanical stress to ~20% of bare silicon, with ultralow surface energy and friction.
  • Identified coating-dependent thresholds in adhesion, friction, and elastic modulus for NIL mold design.

Conclusions:

  • MLD/ALD coatings offer a unified and predictive framework for active interfacial control in NIL.
  • Graphene coatings provide a pathway toward durable molds, efficient demolding, and high-precision nanoscale pattern transfer.
  • Actionable guidelines for coating selection were established for advanced nanomanufacturing.